1 Overview of Ceramic Matrix Composites

Ceramic matrix composites (CMCs) are a class of advanced composite materials prepared with ceramics as the matrix and reinforced with fibers, whiskers, particles, or other reinforcements . As an important branch of advanced ceramics, CMCs inherit the advantages of traditional ceramics such as high hardness, high-temperature resistance, oxidation resistance, and corrosion resistance, while overcoming the shortcomings of traditional ceramics such as high brittleness and easy fracture. They achieve high reliability that is "unbreakable when knocked and unbreakable when dropped," and are known as "shatterproof ceramics." CMCs are typical dual-use strategic emerging materials and engineering materials for both military and civilian applications, with urgent application needs and broad development prospects in aerospace, modern transportation, new energy, and other fields.

IMG20251221104849

Ceramic matrix composites mainly consist of three parts: the ceramic matrix, the reinforcement, and the interface phase.

The ceramic matrix is the main body of the ceramic matrix composite, primarily serving to provide high-temperature resistance, oxidation and ablation resistance, and resistance to environmental erosion. Common matrix materials mainly include carbon matrices, silicon carbide matrices, oxide matrices, and nitride matrices. Carbon matrix composites are mainly used in inert or reducing environments, such as carbon fiber-reinforced carbon matrix composites. Their strength increases with rising temperature, and they have excellent thermal shock resistance, but their oxidation resistance is relatively poor, so oxidation-resistant coatings are usually prepared on the surface. SiC has excellent high-temperature oxidation resistance; in an oxidizing environment, it forms a SiO2 oxide layer that prevents the inner SiC from further oxidative attack. Oxide matrices mainly include alumina, mullite, aluminosilicates, etc. Their main advantage is that they do not have oxidation problems, but their high-temperature creep resistance is relatively poor, and there is thermal expansion coefficient mismatch with some reinforcements. Nitride matrices such as silicon nitride have high hardness, good thermal shock resistance, and relatively high fracture toughness [2].

The introduction of reinforcements is intended to significantly improve the fracture toughness and mechanical strength of ceramic matrix materials, thereby avoiding brittle fracture of ceramic materials under load and achieving superior and more reliable mechanical performance [3]. Reinforcements are mainly divided into continuous reinforcements and discontinuous reinforcements. Currently, the widely used continuous fiber reinforcements are mainly carbon fibers and silicon carbide fibers.

The interface lies between the fiber and the matrix and serves to protect the fiber, achieving toughening effects through crack deflection, interface debonding, and other mechanisms. Commonly used interface phases include pyrolytic carbon interfaces, silicon carbide interfaces, boron nitride interfaces, etc.

2 Preparation Processes of Ceramic Matrix Composites

The preparation methods of ceramic matrix composites mainly include chemical vapor infiltration, slurry infiltration, polymer precursor impregnation and pyrolysis, and reactive melt infiltration. Different preparation methods differ significantly in matrix densification degree, degree of fiber damage, microstructure, and composite properties 

2.1 Chemical Vapor Infiltration (CVI) 

CVI is an extension of chemical vapor deposition. Gaseous precursors are introduced at high temperature into the pores of a porous fiber preform, where they react on the fiber surface to form a solid ceramic matrix that deposits within the preform. By precisely controlling reaction temperature, pressure, and gas composition, densification of the composite from the inside out can be achieved. The advantages of this process are that the reaction temperature during preparation is not high, fiber damage is relatively small, the prepared ceramic matrix has high purity and complete crystal form, and the mechanical properties of the composite are relatively high. The disadvantages are a long manufacturing cycle, high cost, and high porosity in the prepared composite.

2.2 Reactive Melt Infiltration (RMI)

RMI is the process of infiltrating liquid metal into a porous carbon preform, where it reacts chemically with the carbon matrix in the preform to form a ceramic phase, thereby obtaining a ceramic matrix composite. This process has low cost, a short cycle, and rapid densification. The prepared composite has low porosity and relatively high thermal conductivity and airtightness, but there are problems such as low comprehensive mechanical properties, difficulty in controlling the microstructure, and poor creep resistance .

2.3 Precursor Impregnation and Pyrolysis (PIP) 

PIP is a method in which a low-viscosity precursor solution is impregnated into fiber fabrics or porous composites, followed by heating to achieve crosslinking and curing of the polymer, and finally pyrolysis at high temperature to convert the polymer into ceramic. To achieve densification, the PIP process generally requires multiple cycles.

PIP has the advantages of a simple preparation process, strong designability of precursor molecules, relatively low preparation temperature, the ability to prepare complex-shaped components, a simple liquid-phase precursor impregnation process, and easy infiltration into fiber bundles. At the same time, however, it has problems such as low single-cycle yield, high porosity, long PIP cycle time, fiber damage caused by reactive substances and repeated heat treatment, and micropores and microcracks in the matrix caused by volume shrinkage during pyrolysis. At present, PIP methods are developing toward strengthening component design, improving precursor yield, improving impregnation efficiency, and lowering sintering temperature.

2.4 Slurry Infiltration (SI)

In the slurry infiltration method, a high-solids-content ceramic slurry with uniformly dispersed ceramic powder is first obtained by ball milling, and then the ceramic slurry is infiltrated between fiber cloth layers by fiber impregnation or brushing. Next, a preform is obtained by lamination hot pressing or vacuum bag technology. Finally, the preform is sintered at high temperature to obtain a ceramic matrix composite blank [7].

The SI method has a simple process and short cycle, and the resulting composite has relatively high mechanical properties. At the same time, it also has the advantage of near-net shaping and is suitable for preparing components with complex shapes. However, the high temperature and pressure applied during the process can cause fiber damage.

3 Processing Technologies for Ceramic Matrix Composites

Ceramic matrix composites have high hardness, a multiphase structure, and anisotropy, and are prone to forming many defects on the surface during processing, making them typical difficult-to-machine materials. Processing methods for ceramic matrix composites can be divided into traditional mechanical processing and special processing represented by laser processing, ultrasonic processing, water jet processing, etc.

3.1 Traditional Mechanical Processing 

Traditional mechanical processing of ceramic matrix composites mainly includes grinding, milling, drilling, and turning. Research is mainly focused on the selection of tool materials, optimization of process methods, and selection of process parameters.

Traditional mechanical processing technology has high efficiency, simple operation, and low cost, and has become increasingly mature. At present, diamond tools (PCD tools) at home and abroad are the preferred choice for traditional processing of ceramic matrix composites. The problems in process parameters are severe tool wear, low processing efficiency, and poor quality, specifically manifested as poor dimensional consistency, surface cracks, fracture, delamination, fiber debonding, fiber pullout, edge chipping, and other defects, which seriously affect processing quality and surface precision of the material.

3.2 Ultrasonic Vibration-Assisted Machining

Ultrasonic vibration-assisted machining (UVAM) is a new composite processing technology that integrates traditional mechanical processing and ultrasonic technology. It applies controllable high-frequency vibration to the tool or workpiece, changing the contact and interaction state between the tool and the workpiece, and causing periodic contact and separation between the tool and the workpiece. Ultrasonic vibration-assisted machining of ceramic matrix composites can effectively reduce cutting force, reduce the friction coefficient between the tool and the cutting interface, and improve processing efficiency, machined surface quality, and tool life .

3.3 Laser Processing 

The core of laser processing technology lies in using a high-energy-density beam to achieve local energy deposition on the material surface. Through a precision optical system, radiant energy is focused on a microscopic region to accomplish ablation, modification, or joining of the target. This technology avoids tool wear and workpiece deformation problems generated in traditional mechanical processing. By precisely regulating core parameters such as laser power density, pulse width, and repetition frequency, the heat-affected range in the processing area can be effectively suppressed. Laser processing mainly includes continuous laser processing and (picosecond, femtosecond) ultrashort pulse processing. For ceramic matrix composites, compared with continuous laser processing, ultrashort pulse laser processing provides higher material precision, less damage, and better processing results.

3.4 Abrasive Water Jet Machining

Abrasive water jet machining (AWJM) technology uses a high-pressure water pump to pressurize water, converts high-pressure low-flow-rate water into a high-speed jet through a nozzle, and simultaneously adds a certain amount of abrasive to form a liquid-solid two-phase high-speed jet, which impacts the material surface with extremely high kinetic energy to achieve cutting, cleaning, or surface treatment of the material.

Abrasive water jet machining has good application prospects in cutting and drilling of ceramic matrix composites. It has no heat-affected zone, can well preserve the mechanical properties of the material, has high processing efficiency, and is suitable for processing high-hardness components. However, the processing accuracy and surface quality of this technology are insufficient, and the abrasive utilization rate is low. The recovery technology is not mature, and cutting efficiency decreases significantly after recycling .

3.5 Electrical Discharge Machining

Electrical discharge machining refers to a method of processing a workpiece through the electrical erosion effect of pulse discharge between a tool electrode and a workpiece electrode in a certain medium. Electrical discharge machining has the characteristics of relatively high processing accuracy and low tool cost, and is widely used for processing difficult-to-machine materials and complex, tiny geometric structures.

In the electrical discharge machining process, the main material removal modes are cracks caused by thermal diffusion of the matrix material and fracture of insulating fibers. During the removal of the ceramic matrix material, cracks, crack propagation, and spalling occur under the thermal shock of the spark. Due to the thermal shock generated by the spark, the fibers undergo thermal expansion and compression and eventually brittle fracture. Its challenge is that material removal rate is low because of the low electrical conductivity of the workpiece and low debris removal efficiency.

4 Conclusion

Ceramic matrix composites rely on the synergistic toughening mechanism of multiphase components to overcome the brittle defects of traditional ceramics and have irreplaceable application value in extreme service scenarios.

At the material preparation level, a single process is difficult to meet all the requirements of high performance, low cost, complex shapes, and short cycles, so composite processes have become the mainstream development direction. For example, CVI+RMI, CVI+PIP, etc., use CVI to prepare the interface layer to protect the fibers, and then use RMI, PIP, and other methods to achieve rapid densification and forming of complex components. Composite processes can achieve a good balance among ensuring fiber performance, improving densification degree, and reducing preparation cost.

At the processing level, special processing is the main direction for the future development of ceramic matrix composite processing technology. Emphasis should be placed on in-depth exploration of processing mechanisms, research on processing equipment, further optimization of process parameters, and improvement of technologies for detecting and suppressing surface/subsurface damage. In addition, other high-precision, high-efficiency composite and combined process technologies still need to be explored, and research on special processing technologies for rapid manufacturing should be carried out.

Continuously promoting the iterative upgrading of preparation and processing technologies for ceramic matrix composites will strongly support the domestic development of key components for high-end equipment in extreme environments.